Understanding Battery Aging: Charging Scientifically to Extend Battery Life

Battery Aging
  • Whatsapp/Wechat: (+86)18925002618
  • Email: sales@atomemotor.com
  • Headquarters: Washington Business Park 7 Washington Drive Unit 25 Halfway House Midrand
Table of Contents
    Add a header to begin generating the table of contents

    Lithium ion batteries are widely used in electric vehicles, electric motorcycles, power tools and other fields. However, when the battery is used for a long time, it is found that the battery is not durable and needs to be charged frequently, which indicates battery aging.

    What effects will battery aging bring? This article will introduce the battery aging mechanism, battery aging detection and battery scientific charging.

    YouTube_play_button

    Analysis of Battery Aging Mechanism

    Solid electrolyte interface (SEI) layer growth

    What is SEI: The SEI layer is a protective passivation film formed on the surface of the anode of a lithium battery, similar to the oxide film formed by metallic aluminum in the air. It is mainly composed of lithium compounds, such as LiF, Li₂CO₃, etc.

    Formation process: During the first charge, the electrolyte molecules decompose on the surface of the anode to form an initial SEI layer (thickness of about 10nm). This initial layer should protect the anode and prevent further reaction. However, the solvent molecules can still slowly pass through the SEI layer and continue to react on the surface of the anode, causing the SEI to continue to thicken.

    Life example: When you buy a new mobile phone or electric car, the first few charge and discharge cycles (activation process) are actually forming a stable SEI layer. This is the scientific explanation for why new equipment needs “running-in”.

    Influencing factors:

    • Temperature: High temperature environment (such as charging in the summer sun, or placing the device near a heat source) significantly accelerates SEI growth
    • Storage state: High power state (>80%) storage will accelerate SEI growth
    • Time: SEI will grow slowly even if not used (calendar aging)
    • User impact: Battery capacity gradually decreases, and it will age even if not used. This is why electric vehicle batteries that are idle for a long time will “naturally decay”.

    Lithium precipitation and dendrite growth

    Lithium precipitation refers to the process in which lithium ions are not embedded in the anode material, but are reduced to metallic lithium on the surface. This phenomenon is particularly prone to occur in the following situations:

    Trigger conditions:
    Low-temperature fast charging: Using fast charging below 0°C in winter is the most dangerous combination
    High current charging: Ultra-fast charging technology (such as full charge in 30 minutes)
    High SOC charging: Frequent charging to more than 95%

    Life examples: Fast charging of electric bicycles outdoors in winter, or charging electric vehicles with high-power charging piles, may cause lithium precipitation.

    Consequence analysis:

    • The precipitated metallic lithium will react with the electrolyte to form more SEI
    • The partially analyzed lithium will lose electronic connection and form “dead lithium”
    • In severe cases, dendrites may form, penetrate the diaphragm, and cause short circuits and safety accidents

    This explains why the capacity of some electric vehicle batteries drops sharply after fast charging in winter, and why manufacturers usually limit charging power in low temperature environments.

    Changes and decomposition of cathode structure

    Modern lithium battery cathode mostly use materials such as nickel manganese cobalt (NMC) or nickel cobalt aluminum (NCA), which undergo complex structural changes during the charge and discharge process.

    Crystal structure transformation: Under high charge state (>80% SOC), the layered structure begins to transform into spinel and rock salt phase structure

    This phase change causes lithium ion channels to be blocked and capacity to decrease

    Oxygen release:

    • When overcharged, oxygen ions in the lattice may be oxidized and released
    • The released oxygen reacts with the electrolyte to produce gas, causing the battery to swell

    Transition metal dissolution:

    • Nickel, manganese and cobalt ions in the cathode dissolve into the electrolyte
    • These metal ions migrate to the anode, catalyzing SEI growth, forming a vicious cycle

    Life example: When you find that a mobile phone or tablet that has been used for a long time begins to swell, it is likely caused by the decomposition and release of gas from the positive electrode material. Even if the battery has a built-in battery management system, battery manufacturers recommend avoiding long-term high power state.

    Influencing factors:

    • High voltage charging: Charging above 4.2V accelerates structural degradation
    • High temperature environment: High temperature conditions in summer accelerate metal dissolution
    • Charging limit: Limiting charging to 80% can significantly slow this process

    Particle rupture

    Lithium battery electrodes are composed of micron-sized active particles. These particles expand and contract repeatedly during charge and discharge, resulting in internal stress accumulation and rupture.

    Rupture mechanism:
    Lithium ion concentration gradient generates mechanical stress
    Repeated cycles cause fatigue cracks to expand and rupture, exposing new surfaces and accelerating other aging reactions

    Special case – silicon-based anode
    Silicon as a anode additive can greatly increase capacity (theoretically 10 times that of graphite), but the volume expands by up to 300% during charging and is very easy to rupture, which is why pure silicon anode batteries are difficult to commercialize.

    Real life example: High rate charging and discharging of electric vehicles (such as frequent use of DC fast charging or intense driving) will accelerate particle fracture. This is why some electric vehicle manufacturers recommend limiting the frequency of fast charging.

    Crystal structure transformation:

    • Charge and discharge rate: High rate operation accelerates fracture
    • Temperature extremes: Too high or too low temperature will promote fracture
    • Deep cycle: Frequent 0-100% charge and discharge intensifies stress

    Battery Aging Detection and Characterization Technology

    The complexity of battery aging requires advanced detection methods to identify and monitor. Whether researchers are developing new batteries or battery management systems are evaluating battery health status, these technologies are indispensable.

    Electrochemical characterization technology

    • Basic electrochemical measurements:

    Constant current charge and discharge test: the most basic capacity measurement method, recording capacity changes with the number of cycles
    High-precision coulometer (HPC): Identify irreversible capacity loss by accurately measuring charge and discharge power
    Hybrid pulse power test (HPPC): Evaluate internal resistance increase and power attenuation

    • Electrochemical impedance spectroscopy (EIS):

    Measure the impedance response of the battery at different frequencies by applying a small AC signal
    The high-frequency region corresponds to the electrolyte and contact resistance
    The medium-frequency region reflects the charge transfer process and SEI layer impedance
    The low-frequency region corresponds to the solid-state diffusion process
    EIS can separate the impedance contributions from different sources and reveal specific aging mechanisms

    Targeted aging mechanism induction and detection

    SEI layer growth detection:
    Monitoring SEI growth through changes in specific frequency regions in the impedance spectrum
    Tracking SEI mass increase using electrochemical quartz crystal microbalance (EQCM)
    Analyzing gas products during SEI formation using differential electrochemical mass spectrometry (DEMS)

    Lithium precipitation detection:
    Using Arrhenius plot analysis to distinguish between SEI growth and lithium precipitation contributions
    Specific signals in differential voltage analysis for quantitative lithium precipitation
    Lithium precipitation estimation method based on impedance-capacity relationship diagram

    Particle rupture characterization:
    Acoustic emission sensor detects rupture sound waves in real time
    Synchrotron radiation X-ray tomography imaging to observe internal microstructure
    Digital image correlation technology to measure stress-strain relationship
    Indentation test to determine material mechanical properties (Young’s modulus, fracture strength)

    Lithium Battery Scientific Charging and Usage Suggestions

    Based on a deep understanding of the battery aging mechanism, the following are scientific recommendations for extending the lithium ion battery life:

    Daily use recommendations

    Charging habits: Keep the power within the range of 20-80%, avoid frequent full charge or over-discharge. Avoid fast charging in low-temperature winter environments. If necessary, preheat the battery. Use original or qualified chargers and avoid using inferior charging equipment.

    Temperature management: Avoid using or charging in high-temperature environments (such as direct sunlight). Do not force fast charging in an overly cold environment. Avoid the device being in a high-temperature environment for a long time (such as exposure in the car).

    Storage method: Long-term storage (>2 weeks) Keep the power at 40-60%. The ideal storage environment temperature range is 10-25°C. Avoid long-term storage at 0% or 100%.

    Cycle management:
    For electric vehicles: Charge as needed, not full every day.
    For electric bicycles: Avoid charging after full discharge.
    For mobile phones/tablets: Avoid frequent short-term charging (micro-cycles) and avoid connecting the charger for a long time.

    Special recommendations for different devices

    • Electric vehicles:

    Charge to 80% for daily use, and charge to 100% before long-distance travel
    Smart charging: Set the departure time to optimize the charging process for the vehicle
    Try to use slow home charging and limit the frequency of DC fast charging

    • Electric bicycles/electric motorcycles:

    Avoid charging under extreme conditions of high or low temperatures
    Charge promptly after use, but avoid keeping the battery fully charged for a long time
    Preheat properly before charging in winter

    • Mobile phones/tablets/laptops:

    Modern devices have battery management systems, avoid charging to 100%
    Turn on optimized charging functions (such as iPhone’s optimized charging)
    Avoid high-load operations such as playing games while charging

    Conclusion

    Lithium ion battery aging is a complex process with multiple mechanisms, multiple scales, and high coupling. Understanding these mechanisms can help us use batteries more scientifically and extend the life of devices.

    For consumers, proper usage habits can significantly extend battery life; for researchers, a deep understanding of aging mechanisms is the basis for developing the next generation of high-performance, long-life batteries.

    As the wave of electrification advances, the battery types continue to increase, and battery technology will continue to develop, but good usage habits will always be the key to extending battery life.

    Related Posts

    Latest Articles

    Dry Cell Battery

    Understanding Dry Cell Battery: Definition, Types and Storage Methods

    A dry cell battery (Dry battery) is a chemical battery that uses a paste electrolyte to generate direct current, which is different from a wet ...
    Lithium-Ion Battery Failures

    Lithium-Ion Battery Failures: Classification, Mechanisms, and Management

    Lithium-ion battery failure is a complex process. The root cause of failure is irreversible damage to the internal materials and structures of the battery, which ...
    Africa’s E-Motorcycle Boom

    Africa’s E-Motorcycle Boom: China Seizes the Opportunity

    Ethiopia has implemented one of the world's strictest bans on the import of gasoline-powered vehicles. The South African government plans to ban the sale of ...
    Battery Safety Testing

    Understanding Battery Safety Testing: Core Items and Testing Standards

    The core battery safety testing components are divided into four main areas: mechanical safety testing, electrical safety testing, environmental safety testing, thermal runaway testing, and ...
    Deep Cycle Battery

    Understanding Deep Cycle Battery: Application and Selection Guide

    Deep cycle battery is rechargeable batteries capable of long, deep discharge cycles. Unlike conventional batteries, deep cycle batteries can withstand repeated discharges to a lower ...
    Electric Tricycle Battery

    Understanding the Electric Tricycle Battery: Types, Selection, and Maintenance

    The variety of batteries used in electric tricycles is increasing. Currently, the main types of electric tricycle battery include lead-acid batteries, lithium-ion batteries, and sodium-ion ...

    Best Products

    Contact Us

    Have a specific question or request? Fill out the form below, and we’ll get back to you as soon as possible.

    Contact Form Demo
    Scroll to Top

    Talk to us!

    We’ll gladly walk you through the products during a demo and answer any questions! Just drop us a message, we’ll get back to you!

    • Whatsapp/Wechat: (+86)18925002618
    • Email: sales@atomemotor.com
    • Headquarters: Washington Business Park 7 Washington Drive Unit 25 Halfway House Midrand, Johannesburg, South Africa
    • Factory: No. 95, Zongdui Road, Daling Village, Dalingshan, Dongguan, Guangdong, China